Converter Gunning Materials
Type |
Chemical Composition/% |
Ultimate Particle Size/mm |
highest temperature for use/℃ |
Form of Construction |
||||
MgO |
CaO |
C |
SiO2 |
Fe2O3 |
||||
JFFC-G85 |
≥85 |
≤4 |
― |
≤4 |
≤1.6 |
3 |
1800 |
spray gun wet type spray repair |
JFFC-G83 |
≥83 |
≤4 |
― |
≤6 |
≤2 |
3 |
1800 |
|
JFFC-G68 |
63~68 |
≥20 |
― |
≤4 |
3~5 |
3 |
1800 |
|
JFFC-D80 |
≥80 |
― |
≥3 |
≤2 |
≤1.6 |
3 |
1800 |
spray gun dry type spray repair |
JFFC-D77 |
≥77 |
― |
≥3 |
≤5 |
≤2 |
3 |
1800 |
|
Production Introduction |
This product uses high-quality sintered magnesia dolomite sand or sintered magnesia as main raw materials, and is obtained by mixing the composite binder. It has the advantage of high slag resistance, high adhesive rate and smooth operation, which is the ideal material for improving the service life of the converter lining. |
|||||||